Nanoscale , 2015, Advance Article
DOI: 10.1039/C4NR06332E, Paper
DOI: 10.1039/C4NR06332E, Paper
Ziang Zhang, Alex Kutana, Boris I. Yakobson
During graphene fracture under uniaxial load, fully reconstructed zigzag edges can form through sequential atomic rearrangements at the crack tip.
To cite this article before page numbers are assigned, use the DOI form of citation above.
The content of this RSS Feed (c) The Royal Society of Chemistry
During graphene fracture under uniaxial load, fully reconstructed zigzag edges can form through sequential atomic rearrangements at the crack tip.
To cite this article before page numbers are assigned, use the DOI form of citation above.
The content of this RSS Feed (c) The Royal Society of Chemistry